NO Chemisorption on Cu/SSZ-13: A Comparative Study from Infrared Spectroscopy and DFT Calculations

Renqin Zhang, Jean‐Sabin McEwen, Márton Kollár, Feng Gao, Yilin Wang, János Szanyi, Charles H. F. Peden

ACS Catalysis · 2014 · 167 citations · 36 references

Concepts

Abstract

The locations and energies of Cu ions in a Cu/SSZ-13 zeolite catalyst were investigated by density functional theory (DFT) calculations. For “naked” Cu 2+ ions (i.e., Cu 2+ ions with no ligands in their coordination spheres other than zeolite lattice oxygen atoms), the more energetically favorable sites are within a 6-membered ring. However, with the presence of various adsorbates, the energy difference between 6- and 8-membered ring locations greatly diminishes. Specifically, Cu 2+ ions are substantially stabilized by −OH ligands (as [Cu II (OH)] + ), making the extra-framework sites in an 8-membered ring energetically more favorable than 6-membered ring sites. Under fully dehydrated high vacuum conditions with different Si/Al and Cu/Al ratios, three chemisorbed NO species coexist upon exposure of NO to Cu/SSZ-13: NO +, Cu 2+ –NO, and Cu + –NO. The relative signal intensities for these bands vary greatly with Si/Al ratios. The vibrational frequency of chemisorbed NO was found to be very sensitive to the location of Cu 2+ ions. On the one hand, with the aid from DFT calculations, the nature for these vibrations can be assigned in detail. On the other hand, the relative intensities for various Cu 2+ –NO species provide a good measure of the nature of Cu 2+ ions as functions of Si/Al and Cu/Al ratios and the presence of humidity. These new findings cast doubt on the generally accepted proposal that only Cu 2+ ions located in 6-membered rings are catalytically active for NH 3 –SCR.

References

36