Journal of Physics D Applied Physics · 1998 · 12 citations · 14 references
Natural SciencesMaterials EngineeringMaterials ScienceElectronic MaterialsMaterials CharacterizationThin FilmsDielectric PropertiesDielectricsThin Film AnnealingThin Film Electrical PropertiesThin-film DepositionThin-film MaterialsDielectric ConstantFerroelectric PropertiesFerroelectric Thin FilmsPhysical PropertiesPolycrystalline Thin FilmsSiliconThin Film FerroelectricsThin-film Dielectrics
BaTiO 3 thin films have been prepared firstly by an atmospheric-pressure metal-organic chemical vapour deposition technique.Smooth and polycrystalline films with uniform composition were deposited onto silicon substrates at a substrate temperature of 700 C for 1 h and the fully (001)-textured films were obtained with a rapid thermal annealing process thereafter at a temperature of 750 C for 60 s.The prepared films exhibited good structural, dielectric and ferroelectric properties.The measured dielectric constant and dissipation factor at a frequency of 100 kHz were 107 and 0.066, respectively, for a 1.0 m thick film annealed at 750 C for 60 s.The frequency dependences of the dielectric constant () and the dissipation factor (tan ) were also investigated.The ferroelectricity of the films was confirmed by recording P -E hysteresis loops with remnant polarization and coercive field values of 2.0 C cm -2 and 4.0 kV cm -1 , respectively.The Curie temperature (T c ) of the films was found to be 378 K.The influence of stress on the physical properties of the films was investigated.
14
J. F. Scott, Carlos A. Paz de Araújo · Science · 1989 · 3.8K citations
Natural Sciences, Electrical Engineering, Materials Science +17
Metalorganic chemical vapor deposition of BaTiO3 thin films
B. S. Kwak, K. Zhang, E. P. Boyd et al. · Journal of Applied Physics · 1991 · 157 citations
Natural Sciences, Materials Engineering, Materials Science +16