Electrical Conduction in Nb2 O 5 ‐ Doped Cerium Dioxide

I. Naik, T. Y. Tien

Journal of The Electrochemical Society · 1979 · 55 citations · 0 references

Concepts

Abstract

Electrical conductivity of the sintered specimens was measured between 800° and 1329°C in the range 10−19–1 atm. A polarization technique was used to determine the predominant electrical conduction mode in these specimens. Thermogravimetric analysis was done to measure the weight loss in selected specimens. The solid solubility limit of in is between 0.60 and 0.80 m/o, and it does not vary significantly with temperature or . The is an n‐type semiconductor. At high , Nb5+ ions are incorporated in by both possible charge‐compensating mechanisms, viz., (i) reduction of some Ce4+ to Ce3+ and (ii) formation of oxygen interstitials. At low , the first mechanism predominates. Doping with significantly increases the electrical conductivity of in the high range. This extrinsic electronic conductivity, arising from mechanism (i), predominates over the intrinsic conductivity at high (10−4–1 atm) and lower temperatures (800°–1029°C) giving total conductivity at a constant temperature. At lower or higher temperature, the intrinsic defects of increasingly affect the conductivity.