Japanese Journal of Applied Physics · 1966 · 15 citations · 7 references
Natural SciencesMaterials EngineeringMaterials ScienceElectronic MaterialsSemiconductor MaterialsSolid State PhysicsAlloysCrystal ChemistryDopingInorganic MaterialsSemiconductor Crystal GrowthSemiconductor Device MaterialsBridgman GrowthCarrier ConcentrationDistribution CoefficientElectrical PropertiesElectrical Properties AnalysisSolid Solubility LimitSolubilityX-ray Diffraction Analysis
The phase diagram for the Bi 2 Te 3 -Ge system in the region of 0–6 atomic percent Ge was determined by thermal analysis, X-ray diffraction, and the study of crystal growth. The solubility limit of Ge in solid Bi 2 Te 3 was found to be about 0.3%, and the distribution coefficient to be about 0.1. Crystals containing various amounts of Ge up to the solubility limit were prepared by the Bridgman method. The electrical properties of Bi 2 Te 3 are not much affected by the addition of Ge, and hence Ge is regarded as practically inactive in Bi 2 Te 3 . The secondary solid solution of the Bi 2 Te 3 -Ge system, which contains more than 1.2% Ge, is an n -type semiconductor with a very high carrier concentration (of the order of 10 20 cm -3 ). The crystal growth study shows that most of Ge-doped specimens used in Bergmann's works were highly inhomogeneous.
7
The redistribution of solute atoms during the solidification of metals
William A. Tiller, Kenneth A. Jackson, J. W. Rutter et al. · Acta Metallurgica · 1953 · 1.7K citations
W. G. Pfann · JOM · 1952 · 238 citations