Journal of Applied Physics · 1997 · 213 citations · 11 references
Natural SciencesMaterials EngineeringMaterials ScienceElectronic MaterialsSemiconductor MaterialsThin FilmsSemiconductor Device MaterialsSemiconductor Thin FilmsSolar Cell MaterialsSolar CellsSurface PhysicsThin-film MaterialsAnnealingEnergy Dispersive X-ray SpectroscopyEnergy-dispersive X-ray SpectroscopyPrecursor MaterialsSputteringSputtering ProcessesSputtering TechniquesX-ray Diffraction Analysis
CuIn x Ga 1−x Se 2 thin films, with various Ga/(Ga+In) ratios, suitable for solar cells were processed by selenizing stacked Cu, Ga, and In precursor layers in a H2Se reactor in the temperature range of 400–500 °C. Cu/Ga/In and Cu/In/Ga precursors were obtained by sequential sputtering of the elemental layers. The Cu/Ga/In and Cu/In/Ga precursors, and the selenized films were characterized by scanning electron microscopy, x-ray diffraction, energy dispersive spectroscopy, and Auger electron spectroscopy. The precursors contained only binary and elemental phases in the as-deposited condition and after annealing. The selenized films had a nonuniform distribution of Ga and In. The surface of the selenized films were In rich, while the Mo/film interface in these films was Ga rich. The selenized films with Ga/(Ga+In) ratios greater than 0.25 contain graded Ga and In compositions, and the selenized films with Ga/(Ga+In) ratios less than 0.6 contain a phase-separated mixture of CuInSe2 and CuGaSe2 with the CuInSe2 near the surface and the CuGaSe2 near the Mo/film interface. Single phase, homogeneous CuInxGa1−xSe2 films were obtained by annealing the as-selenized films in argon in the temperature range of 500–600 °C for 60 min. Interdiffusion of In and Ga between the CuGaSe2 and the CuInSe2 phases was found to be responsible for the homogenization process. This homogenization process does not occur in the presence of a selenium atmosphere. Diffusion measurements yielded similar interdiffusion coefficients for Ga and In. The annealing temperature and time to effect homogenization depends on the Ga/(Ga+In) ratio of the absorber films. Films with lower Ga/(Ga+In) ratios require a homogenization temperature of 600 °C or more and films with higher Ga/(Ga+In) ratios homogenize at a lower temperature of 400–500 °C, for an annealing time of 60 min.
11
CuInSe2 for photovoltaic applications
Angus Rockett, Robert W. Birkmire · Journal of Applied Physics · 1991 · 445 citations
An introduction to solid state diffusion
Choice Reviews Online · 1989 · 382 citations
Transport properties of CuInSe2
S. M. Wasim · Solar Cells · 1986 · 222 citations
Phase Diagram and Optical Energy Gaps for CuInyGa1−ySe2 Alloys
T. Tinoco, Carlos Rincón, M. Quintero et al. · physica status solidi (a) · 1991 · 116 citations
Natural Sciences, Materials Engineering, Materials Science +17