Development of a sustainable engineered geopolymer composite with mitigated autogenous shrinkage, enhanced mechanical performance, and improved thermal behaviour by recycled concrete powder

Yuekai Xie, Yingying Guo, Jianfeng Xue

Powder Technology · 2025 · 23 citations · 42 references

DOIFull text

Open access

Concepts

Abstract

The application of recycled concrete powder (RCP) into engineered geopolymer composites (EGC) could be a sustainable alternative to decreasing the carbon footprint and improving the mechanical properties of EGC. This paper evaluated the mechanical properties, autogenous shrinkage, thermal resistance, and microstructures of RCP-EGC. The results indicated that the replacement of natural sand (NS) with RCP decreased the autogenous shrinkage of RCP-EGC by up to 19.1 %. With partial replacement of NS with RCP (75 %), the compressive strength was increased from 66.6 to 77.7 MPa and slightly decreased to 76.8 MPa with complete replacement. The 100 % replacement of NS with RCP increased the tensile strength and strain capacity from 4.93 to 6.25 MPa, and 9.26 % to 11.14 %, respectively. The improvement in the mechanical behaviour was attributed to the enhanced gel formation, as can be verified by the microstructural results. After thermal exposure to 60 and 120 °C, RCP-EGC with 100 % RCP exhibited enhanced compressive strength (87.4 MPa), tensile strength (7.18 MPa), and strain capacity of (10.44 %), higher than those without RCP (73.3 MPa, 5.45 MPa, and 8.15 %). For the samples exposed to 180 °C, the strain-hardening behaviour could not be determined. The RCP-EGC exhibited higher compressive strength after the higher thermal exposure of 180, 300 and 400 °C. The results from carbon footprint calculation and cost-effectiveness analysis suggested replacing NS with RCP can be an environmentally friendly and economically affordable alternative to improving the behaviour of EGC at ambient and elevated temperatures. • Use recycled concrete powder (RCP) for engineered geopolymer composite (EGC). • RCP decreased 28-day autogenous shrinkage of EGC from 3921 to 3172 με. • RCP enhanced the strain capacity of EGC from 9.26 % to 11.14 %. • RCP-EGC exhibited improved mechanical performance at 60 to 400 °C than pure EGC. • RCP-EGC could be a cost-effective and environmentally friendly product.

References

42