Journal of Advanced Ceramics · 2022 · 40 citations · 45 references
Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsCorrosion ScienceSurface ScienceAlloysCoatingsCorrosion EngineeringCorrosion MechanismsCorrosion ResistanceCorrosion-resistant MaterialsBarrier CoatingsCorrosion BehaviorCorrosion-resistance MechanismsOxidationSurface Pre-oxidationSurface Roughness Effects On CorrosionThermal Barrier CoatingsTitanium Alloys
Abstract Calcium-magnesium-alumina-silicate (CMAS) corrosion is a serious threat to thermal barrier coatings (TBCs). Ti 2 AlC has been proven to be a potential protection layer material for TBCs to resist CMAS corrosion. In this study, the effects of the pellet surface roughness and temperature on the microstructure of the pre-oxidation layer and CMAS corrosion behavior of Ti 2 AlC were investigated. The results revealed that pre-oxidation produced inner Al 2 O 3 layer and outer TiO 2 clusters on the pellet surfaces. The content of TiO 2 decreased with decreasing pellet surface roughness and increased along with the pre-oxidation temperature. The thickness of Al 2 O 3 layer is also positively related to the pre-oxidation temperature. The Ti 2 AlC pellets pre-oxidized at 1050 °C could effectively resist CMAS corrosion by promoting the crystallization of anorthite (CaAl 2 Si 2 O 8 ) from the CMAS melt rapidly, and the resistance effectiveness increased with the pellet surface roughness. Additionally, the CMAS layer mainly spalled off at the interface of CaAl 2 Si 2 O 8 /Al 2 O 3 layer after thermal cycling tests coupled with CMAS corrosion. The Al 2 O 3 layer grown on the rough interface could combine with the pellets tightly during thermal cycling tests, which was attributed to obstruction of the rough interface to crack propagation.
45
Overview on advanced thermal barrier coatings
Robert Vaßen, Maria Ophelia Jarligo, T. Steinke et al. · Surface and Coatings Technology · 2010 · 1.2K citations