MATERIALS TRANSACTIONS · 2002 · 28 citations · 11 references
Natural SciencesMaterials EngineeringMaterials ScienceMaterials CharacterizationMechanical Behavior Of MaterialsMetallurgyAlloysEutectic TransformationsMetal MaterialsMetalsPhysical MetallurgyThermal Properties Of MaterialsBinary Eutectic AlloysCopper AlloysEndothermic TransitionsEutectic Growth KineticsEutectic Melting BehaviorIntermetallic FormationSolid Solution FormationTensile Strength
The effect of Au addition on the microstructural and the tensile properties of Sn–0.7 mass%Cu alloy was examined. Tensile strength and 0.2% proof stress remarkably increase up to 0.3 mass%Au primarily due to solid solution hardening. Beyond 0.3 mass%Au, due to precipitation of large intermetallic compounds, elongation decreases while tensile strength and 0.2% proof stress increase slightly. With Au addition to Sn–Cu binary alloy, the eutectic endothermic peak in DSC, i.e., the melting reaction at 227°C, becomes broader and shifts to the lower temperature range. With Au beyond 2 mass%, the broad peak becomes smaller splitting into two peaks and moving towards lower temperature while a new peak appears at about 212°C. These thermal reactions can be well explained by the formation of β-Sn, Cu6Sn5 and AuSn4 with Au more than 1 mass%. EPMA observation revealed that much amount of Au and Cu dissolve into Cu6Sn5 and AuSn4, respectively.
11