Progress in Natural Science Materials International · 2022 · 19 citations · 18 references
Natural SciencesMaterials EngineeringMaterials ScienceMechanical Behavior Of MaterialsMetallurgyStructural MaterialsAlloysGrain GrowthHigh-temperature MaterialsMetalsMicrostructure ControlThermal Properties Of MaterialsHigh-temperature Mechanical BehaviorHigh-temperature Mechanical PropertiesPrecipitation StrengtheningShape-memory AlloysStrain RecoveryThermal CyclingUltimate Tensile StrengthYield Stress
The microstructure of the Ti–V–Al shape memory alloy with refined grain and in-situ TiB phase was modified by doping minor Boron (B), which contributes to the superior mechanical performances and strain recovery characteristics. Compared with other quaternary Ti–V–Al-X alloys, the Ti–V–Al–B alloy showed the largest ultimate tensile stress due to the solution strengthening, grain refinement and precipitation strengthening of in-situ TiB phase. Moreover, the Ti–V–Al alloy added 0.1 at.%B possessed the maximum yield stress of 701 MPa and the largest tensile fracture strain of 27.6% at the temperature of 150 °C. Meanwhile, the excellent strain recovery characteristics with fully recoverable strain of 4% could be obtained due to B addition. Besides, B addition suppressed the precipitation of ω phase during thermal cycling and further improved the thermal cycling stability of the Ti–V–Al alloy.
18
Microstructure and shape memory effect of Ti–20Zr–10Nb alloy
Yan Cui, Yan Li, Kun Luo et al. · Materials Science and Engineering A · 2009 · 113 citations
Natural Sciences, Materials Engineering, Materials Science +13