Journal of Power Sources · 2021 · 140 citations · 36 references
EngineeringMaterials EngineeringMaterials ScienceElectrochemical EngineeringElectrochemistryEnergy MaterialsBattery TechnologyBattery TestingElectrochemical CellsElectrochemical Energy StorageElectrode MaterialsEnergy StorageElectrochemical ConductivityIon PlatingLithium DepositsLithium PlatingLithium-ion BatteriesPlatingPulse SequencesPulse Testing
Commercial lithium ion cells with different power: energy ratios were disassembled, to allow the electrochemical performance of their electrodes to be evaluated. Tests on coin cell half cells included rate tests (continuous and pulsed), resistance measurements, and extended pulse tests. Pulse power tests at high rates typically showed three limiting processes within a 10 s pulse; an instantaneous resistance increase, a solid state diffusion limited stage, and then electrolyte depletion/saturation. On anodes, the third process can also be lithium plating. Most of the cells were rated for a 10 C continuous discharge, and the cathode charging voltage at 10 C was around 4.2 V. For anodes, the maximum charge current to avoid a negative voltage was 3–5 C. Negative anode voltages do not necessarily mean that lithium plating has occurred. However, lithium deposits were observed on all the anodes after 5000 pulse sequences with 10 s pulses at ± 20 C.
36
Choice Reviews Online · 2004 · 1.9K citations
Thermodynamic and Mass Transport Properties of “ LiAl ”
Ching-ju Wen, Bernard A. Boukamp, R HUGGINS et al. · Journal of The Electrochemical Society · 1979 · 878 citations