Natural SciencesMaterials EngineeringMaterials ScienceBiocompatibilityMaterials CharacterizationMechanical Behavior Of MaterialsComposite MaterialsMechanical SensorsMems MaterialsNanocompositesSoft SensorsStrain SensorsElasticityElectrical PropertiesPiezoresistive MaterialsPiezoresistive SensingPiezoresistive SensorsPiezoresistive Strain SensorsTensile StrengthYoung's Modulus
The CNT-PDMS composite has been widely adopted in flexible devices due to its high elasticity, piezoresistivity, and biocompatibility. In a wide range of applications, CNT-PDMS composite sensors were used for resistive strain measurement. Accordingly, the percolation threshold 2%~4% of the CNT weight ratio in the CNT-PDMS composite was commonly selected, which is expected to achieve the optimized piezoresistive sensitivity. However, the linear range around the percolation threshold weight ratio (2%~4%) limits its application in a stable output of large strain (>20%). Therefore, comprehensive understanding of the electromechanical, mechanical, and electrical properties for the CNT-PDMS composite with different CNT weight ratios was expected. In this paper, a systematic study was conducted on the piezoresistivity, Young's modulus, conductivity, impedance, and the cross-section morphology of different CNT weight ratios (1 to 10 wt%) of the CNT-PDMS composite material. It was experimentally observed that the piezo-resistive sensitivity of CNT-PDMS negatively correlated with the increase in the CNT weight ratio. However, the electrical conductivity, Young's modulus, tensile strength, and the linear range of piezoresistive response of the CNT-PDMS composite positively correlated with the increase in CNT weight ratio. Furthermore, the mechanism of these phenomena was analyzed through the cross-section morphology of the CNT-PDMS composite material by using SEM imaging. From this analysis, a guideline was proposed for large strain (40%) measurement applications (e.g., motion monitoring of the human body of the finger, arm, foot, etc.), the CNT weight ratio 8 wt% was suggested to achieve the best piezoresistive sensitivity in the linear range.
47
Fully integrated wearable sensor arrays for multiplexed in situ perspiration analysis
Wei Gao, Sam Emaminejad, Hnin Yin Yin Nyein et al. · Nature · 2016 · 4.9K citations · Full text
Sensitive electromechanical sensors using viscoelastic graphene-polymer nanocomposites
Conor S. Boland, Umar Khan, Gavin Ryan et al. · Science · 2016 · 812 citations · Full text
Natural Sciences, Materials Engineering, Materials Science +17