Journal of the Ceramic Society of Japan · 2020 · 10 citations · 13 references
Natural SciencesMaterials EngineeringMaterials ScienceCrystal StructureMaterials ChemistryThin FilmsThin-film DepositionThin-film MaterialsCrystal Surface MorphologyDielectric ConstantFilm ThicknessFilm Thickness ControlHydrothermal ProcessingPiezoelectric PropertiesThin Film CeramicsThin Film Ferroelectrics
(K,Na)NbO3 thick films were prepared at 240 °C on (100)cSrRuO3//(100)SrTiO3 substrates by hydrothermal method. Film thickness increased using an amorphous niobium source instead of conventionally used crystalline one and have the maximum thickness at 0.5 mmol of input mass of niobium source within the range of 0.02–7.5 mmol in case of the 20 h deposition. The yield of (K,Na)NbO3 films from 0.5 mmol amorphous niobium source becomes 20 times higher than that from conventionally used a 2 mmol crystalline niobium source. In addition, crystal structure, surface morphology, dielectric constant, and ferroelectric and piezoelectric properties of these films were almost independent of the kinds of niobium sources and their input mass within the limitation of the present results.
13
notRoles of lattice distortion in (1−x)(Bi0.5Na0.5)TiO3-xBaTiO3 ceramics
Y. S. Sung, J. M. Kim, J. H. Cho et al. · Applied Physics Letters · 2010 · 115 citations
Natural Sciences, Materials Engineering, Materials Science +16