Do Different Application Modes Improve the Bonding Performance of Self-etching Ceramic Primer to Lithium Disilicate and Feldspathic Ceramics?

Quintero-Calderon As, F Siqueira, Michel Wendlinger, Camilo Pulido, María José Masson, Sarmiento-Delgado Ml, Alessandro Dourado Loguércio

PubMed · 2019 · 22 citations · 19 references

Abstract

Active and prolonged application of MEP may be a viable alternative to HF+SI for increasing the bond strength to LD.