Journal of the American Ceramic Society · 2019 · 25 citations · 39 references
Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsCeramicsMechanical Behavior Of MaterialsCeramic CompositesCoating TechnologyCoatingsComposite MaterialsNanocompositesStructural CeramicsBondingCeramic CoatingsShock ResistanceSilicon Carbide CompositesStructural Ceramic CompositesThermal CyclesThermal ShockThermal Shock Resistance
Abstract Mullite coating, SiC whiskers toughened mullite coating (SiC w ‐mullite), and cristobalite aluminum phosphate ( c ‐AlPO 4 ) particle modified SiC w ‐mullite coating ( c ‐AlPO 4 ‐SiC w ‐mullite) were prepared on SiC coated C/SiC composites using a novel sol‐gel method combined with air spraying. Results show that molten SiO 2 formed by the oxidation of SiC whiskers and molten c ‐AlPO 4 improved the bonding strength between mullite outer coating and SiC–C/SiC composites due to their high‐temperature bonding properties. The bonding strength between mullite, SiC w ‐mullite, c ‐AlPO 4 ‐SiC w ‐mullite outer coatings and SiC–C/SiC composites were 2.41, 4.31, and 7.38 MPa, respectively. After 48 thermal cycles between 1773 K and room temperature, the weight loss of mullite/SiC coating coated C/SiC composites was up to 11.61%, while the weight losses of SiC w ‐mullite/SiC and c ‐AlPO 4 ‐SiC w ‐mullite/SiC coatings coated C/SiC composites were reduced to 7.40% and 5.12%, respectively. The addition of appropriate SiC whiskers can considerably improve the thermal shock resistance of mullite coating owing to their excellent mechanical properties at high temperature. In addition, c ‐AlPO 4 particles can further improve the thermal shock resistance of SiC w ‐mullite coating due to their high‐temperature bonding and sealing properties. No obvious micro‐pores and cracks were observed on the surface of c ‐AlPO 4 ‐SiC w ‐mullite coating after 48 thermal cycles due to timely healing effect by formation of secondary mullite.
39
Gaigai Duan, Hong Fang, Shaohua Jiang et al. · Journal of Materials Science · 2018 · 155 citations
Natural Sciences, Materials Engineering, Materials Science +15
SiC whisker-toughened SiC oxidation protective coating for carbon/carbon composites
Hejun Li, Qiangang Fu, Xiaohong Shi et al. · Carbon · 2005 · 78 citations
Natural Sciences, Materials Engineering, Materials Science +12