Formation of Iron-Rich Intermetallic Phases in Al-7Si-Mg: Influence of Cooling Rate and Strontium Modification

Jorge Santos, Anders E. W. Jarfors, A. K. Dahle

Metallurgical and Materials Transactions A · 2019 · 24 citations · 49 references

DOIFull text

Open access

Concepts

Abstract

Abstract The influence of cooling rate on the formation of iron-rich intermetallic phases during solidification of unmodified and strontium-modified Al-7Si-0.3Mg alloys has been investigated. The effect of strontium on the intermetallic phases was evaluated in unquenched and quenched samples. Samples were quenched before the start of the Al-Si eutectic reaction, along the Al-Si eutectic reaction and just after the end of solidification. The results show that the addition of strontium increased the size of both β -Al 5 FeSi and π -Al 8 FeMg 3 Si 6 at low cooling rates. For unmodified and strontium-modified alloys, an increase of cooling rate resulted in a decrease in size of the intermetallic phases, particularly in the strontium modified alloy. In the strontium modified alloy quenched before the start of the Al-Si eutectic reaction, π -Al 8 FeMg 3 Si 6 appeared as thin platelets at the eutectic cell boundaries. Chinese script-like π -Al 8 FeMg 3 Si 6 and platelet-like β -Al 5 FeSi intermetallic phases were observed uniformly distributed in the eutectic regions in the unmodified alloy quenched before the start of the eutectic reaction. Strontium modified semi-solid Al-7Si-0.3Mg castings were produced and the type of intermetallic phase, morphology, size, area fraction and distribution were similar to that observed in the strontium modified alloy quenched before the start of the Al-Si eutectic reaction.

References

49