Zeitschrift für Naturforschung B · 2002 · 28 citations · 0 references
Natural SciencesMaterials SciencePhysicsCondensed Matter PhysicsCrystal StructureMagnetic MaterialsAlloysCrystal ChemistryMagnetic Properties Of SolidsMagnetism Of Inorganic CompoundsX-ray CrystallographyX-ray DiffractionCrystal TwinningMagnetic PropertiesPowder X-ray DiffractionTernary CompoundsTwinningTwinning SymmetryX-ray Diffraction AnalysisZirconia
Single crystals of the ternary indide CeNiIn 2 were synthesized from an indium flux. An arc-melted button of the starting composition CeNiIn 2 was annealed in a zirconia crucible with a slight excess of indium at 1200 K followed by slow cooling (5 K/h) to 870 K. The new indide has been investigated by X-ray diffraction on powders and single crystals: PrNiIn 2 type, Cmcm, a = 440.78(4), b = 1834.3(1), c = 2178.8(2) pm, wR2= 0.0753 for 1471 F 2 values and 66 variable parameters. The structure contains three crystallographically independent nickel positions which have a distorted trigonal prismatic coordination. The CeNiIn 2 structure is related to the MgCuAl 2 structure by chemical twinning. The shortest interatomic distances occur for Ni-In and In-In contacts. The nickel and indium atoms form a complex three-dimensional [NiIn 2 ] network in which the cerium atoms fill distorted pentagonal channels. Magnetic susceptibility measurements indicate Curie-Weiss behavior with an experimental magnetic moment of 2.44(3) μ B /Ce atom. At 3.4(3) K CeNiIn 2 orders ferro- or ferrimagnetically. The experimental saturation magnetization at 2K and 5.5 T is 0.95(2) μ B /Ce.