Inorganic Chemistry · 2012 · 12 citations · 17 references
Natural SciencesChemistryMaterials ScienceCrystal StructureInorganic ChemistryMaterials ChemistryCrystal ChemistryMetal OxidesMineral ChemistryX-ray CrystallographyX-ray DiffractionIn Situ X-ray DiffractionOxidation MechanismsOxide StructurePowder DiffractionPowder Neutron DiffractionPowder X-ray DiffractionTitanium OxidesX-ray Diffraction Analysis
The novel oxide defect fluorite phase ScTiO(3.5) is formed during the topotactic oxidation of ScTiO(3) bixbyite. We report the oxidation pathway of ScTiO(3) and structure evolution of ScTiO(3.5), Sc(4)Ti(3)O(12), and related scandium-deficient phases as well as high-temperature phase transitions between room temperature and 1300 °Cusing in-situ X-ray diffraction. We provide the first detailed powder neutron diffraction study for ScTiO(3). ScTiO(3) crystallizes in the cubic bixbyite structure in space group Ia3 (206) with a = 9.7099(4) Å. The topotactic oxidation product ScTiO(3.5) crystallizes in an oxide defect fluorite structure in space group Fm3m (225) with a = 4.89199(5) Å. Thermogravimetric and differential thermal analysis experiments combined with in-situ X-ray powder diffraction studies illustrate a complex sequence of a topotactic oxidation pathway, phase segregation, and ion ordering at high temperatures. The optimized bulk synthesis for phase pure ScTiO(3.5) is presented. In contrast to the vanadium-based defect fluorite phases AVO(3.5+x) (A = Sc, In) the novel titanium analogue ScTiO(3.5) is stable over a wide temperature range. Above 950 °C ScTiO(3.5) undergoes decomposition with the final products being Sc(4)Ti(3)O(12) and TiO(2). Simultaneous Rietveld refinements against powder X-ray and neutron diffraction data showed that Sc(4)Ti(3)O(12) also exists in the defect fluorite structure in space group Fm3m (225) with a = 4.90077(4) Å. Sc(4)Ti(3)O(12) undergoes partial reduction in CO/Ar atmosphere to form Sc(4)Ti(3)O(11.69(2)).
17
C.N.R. Rao · Annual Review of Physical Chemistry · 1989 · 363 citations
Oxide-ion conductors by design
John B. Goodenough · Nature · 2000 · 314 citations
Natural Sciences, Materials Engineering, Materials Science +12
Temperature-induced magnetization reversal in a YVO3 single crystal
T. T. M. Palstra, D. I. Khomskii, E. Pellegrin et al. · Nature · 1998 · 296 citations · Full text