Journal of Prosthodontics · 2019 · 26 citations · 21 references
DentistryMaterials EngineeringMaterials ScienceCeramic MaterialsCeramicsDental MaterialsAll-ceramic RestorationsCeramic BiomaterialsCeramic BondingCeramic RestorationsDental CeramicsMetal-ceramic SystemsBendingBond StrengthBondingBonding Strength MeasurementFeldspathic CeramicsFracture SurfacesMetal-ceramic Bond StrengthSelective Laser Melting
Abstract Purpose To investigate the effect of bonding agent on the bonding strength between Co‐Cr dental alloy, prepared by selective laser melting (SLM), and feldspathic porcelain. Materials and Methods The experiments were conducted according to ISO 9693 and the conventional protocols for the production of metal‐ceramic dental restorations. After Al 2 O 3 air‐particle abrasion, metal substrates of Co‐Cr dental alloy specimens were bonded, using bonding agent (25 specimens), with dental porcelain positioned in layers (opaque, dentin, enamel). Control specimens (25) were also produced without bonding agent. Bonding strength was measured using 3‐point bending tests, and the results were statistically analyzed using the t‐test and Weibull statistics. Elemental (by SEM/EDS) and crystallographic analyses (by XRD) were conducted on the bonding agent, along cross sections of alloy‐porcelain interfaces, and on fracture surfaces. Results Cohesive fracture occurred (on the porcelain side). The application of the bonding agent decreased the average bonding strength (from 42.27 ± 5.85 to 36.25 ± 3.26 MPa, P = 0.00006), attributed to the nonexisting reaction between the TiO 2 ‐rich bonding agent and the Co‐Cr alloy, but it increased the Weibull modulus (from 7.84 to 12.16), which reflects the reliability of the bond in the tested metal‐ceramic specimens. Conclusions Although the application of bonding agent slightly decreased the bonding strength, all the measured values of the metal‐ceramic specimens produced by the SLM technique, with or without the bonding agent, are markedly higher than the minimum value required by ISO 9693 (25 MPa). Moreover, the use of bonding agent favors the increase of the Weibull modulus.
21
American Journal of Orthodontics · 1961 · 1.8K citations
Cr, Mo and W alloying additions in Ni and their effect on passivity
A. C. Lloyd, James J. Noël, Stewart McIntyre et al. · Electrochimica Acta · 2004 · 281 citations
Natural Sciences, Materials Engineering, Materials Science +10