International Journal of Applied Ceramic Technology · 2019 · 46 citations · 22 references
Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsCeramicsMaterials ChemistryCeramic TechnologySilicon MaterialsSinteringStructural CeramicsThermal Properties Of CeramicsThermal Properties Of MaterialsSiliconSilicon NitrideSilicon Nitride CeramicsSintering BehaviorSintering Effects On Thermal PropertiesSintering ReactionsThermal ConductivityThermally Conductive Ceramics
Abstract Silicon nitride ceramics were pressureless sintered at low temperature using ternary sintering additives (TiO 2 , MgO and Y 2 O 3 ), and the effects of sintering aids on thermal conductivity and mechanical properties were studied. TiO 2 –Y 2 O 3 –MgO sintering additives will react with the surface silica present on the silicon nitride particles to form a low melting temperature liquid phase which allows liquid phase sintering to occur and densification of the Si 3 N 4 . The highest flexural strength was 791(±20) MPa with 12 wt% additives sintered at 1780°C for 2 hours, comparable to the samples prepared by gas pressure sintering. Fracture toughness of all the specimens was higher than 7.2 MPa·m 1/2 as the sintering temperature was increased to 1810°C. Thermal conductivity was improved by prolonging the dwelling time and adopting the annealing process. The highest thermal conductivity of 74 W/(m∙K) was achieved with 9 wt% sintering additives sintered at 1810°C with 4 hours holding followed by postannealing.
22
Silicon Nitride and Related Materials
Frank L. Riley · Journal of the American Ceramic Society · 2000 · 1.5K citations
A Tough Silicon Nitride Ceramic with High Thermal Conductivity
You Zhou, Hideki Hyuga, Dai Kusano et al. · Advanced Materials · 2011 · 333 citations
Development of high-thermal-conductivity silicon nitride ceramics
You Zhou, Hideki Hyuga, Dai Kusano et al. · Journal of Asian Ceramic Societies · 2015 · 163 citations · Full text