Materials Research Express · 2019 · 29 citations · 22 references
Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsCeramicsMechanical Behavior Of MaterialsComposite MaterialsComposites ManufacturingMachiningPowder ProcessingSinteringThermal Properties Of CeramicsSilicon Carbide (Sic) MaterialsSilicon Carbide CompositesSintering Of Ceramic CompositesThermal ShockThermal Shock Resistance
The goal of this research is to investigate the thermal shock resistance of ZrB 2 -30 vol% SiC, consolidated by spark plasma sintering (SPS). So, ZrB 2 and SiC powders were mixed with high energy mill for different milling time of 3, 9 and 15 h. Then sintering process was done for different soaking times (4, 8 and 12 min) and temperatures (1600, 1700 and 1800 °C) under the 40 MPa pressure. Thermal shock resistance was evaluated by water quenching method. The samples were placed in the furnace at various temperatures of 450 ° C to 1600 °C, then cooled down in the water quickly. Flexural strength determined by three-point bending test before and after thermal shock cycle. The morphology of fracture was studied by scanning electron microscopy (SEM). According to the result, with the increase in the SPS temperature, the grain size was increased to some extent, and the microstructure was improved. Flexural strength increased due to porosity reduction, and the thermal shock resistance increased. Increasing the soaking time led to reduction in the flexural strength and thermal shock resistance. Finally, it was cleared that the milling ascent, improved the thermal shock resistance.
22
Zhi Wang, Sai Wang, Xinghong Zhang et al. · Journal of Alloys and Compounds · 2009 · 119 citations
Natural Sciences, Materials Engineering, Materials Science +16