ACS Applied Materials & Interfaces · 2019 · 102 citations · 55 references
Elemental Si has a high theoretical capacity and has attracted attention as an anode material for high energy density lithium-ion batteries. Rapid capacity fading is the main problem with Si-based electrodes; this is mainly because of a massive volume change in Si during lithiation-delithiation. Here, we report that combining an ionic-liquid electrolyte with a charge capacity limit of 1000 mA h g<sup>-1</sup> significantly suppresses Si volume expansion, improving the cycle life. Phosphorus-doping of Si also enhances the suppression and increases the Li<sup>+</sup> diffusion coefficient. In contrast, the Si layer expands significantly in an organic electrolyte even with the charge capacity limit and even in an ionic-liquid electrolyte without the limit. We demonstrated that the homogeneously distributed Si lithiation-delithiation, phase-transition control from the Si to Li-rich Li-Si alloy phases, formation of a surface film with structural and/or mechanical stability, and faster Li<sup>+</sup> diffusion contribute to suppressing Si volume expansion.
55
Issues and challenges facing rechargeable lithium batteries
J. M. Tarascon, Michel Armand · Nature · 2001 · 20.3K citations
Michel Armand, J.-M. Tarascon · Nature · 2008 · 19K citations
Challenges for Rechargeable Li Batteries
John B. Goodenough, Youngsik Kim · Chemistry of Materials · 2009 · 10.6K citations
Size-Dependent Fracture of Silicon Nanoparticles During Lithiation
Shan Huang, Scott X. Mao, Ting Zhu et al. · ACS Nano · 2012 · 2.3K citations
The distillation and volatility of ionic liquids
Martyn J. Earle, José M. S. S. Esperança, Manuela A. Gîlea et al. · Nature · 2006 · 2.1K citations