Journal of Applied Polymer Science · 2018 · 19 citations · 30 references
Natural SciencesMaterials SciencePolymer ChemistryPolymer EngineeringPolymer MaterialsAdhesive BondingBio-based MaterialsPolymer AdhesionThermosetsAdhesion PropertiesAdhesive MaterialsAdhesivesBondingFormaldehydePolymer AdhesivesTensile StrengthUltimate Tensile Strength
Highly phenol substituted bio‐oil–phenol–formaldehyde (BPF) adhesives were prepared via the phenolization‐copolymerization method, in which furfural was used as a novel crosslinking agent to improve the bonding performance. The effects of bio‐oil percentage, furfural content, curing temperature, and pressure on the performance of BPF adhesives have been studied in detail. A BPF adhesive with 75% bio‐oil percentage and 15% furfural loading (named 75BPF_15) was synthesized, which was cured at 180 °C and 4 MPa. Compared to the conventional phenol–formaldehyde adhesive, the wet tensile strength of 75BPF_15 adhesive reached 2.84 MPa, which was significantly higher than the 1.54 MPa of PF. A possible mechanism of BPF adhesives crosslinked with furfural is proposed. © 2018 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2019 , 136 , 46995.
30
David J Chadderdon, John E. Matthiesen, Yang Qiu et al. · Journal of the American Chemical Society · 2017 · 372 citations · Full text
Bio-oil production from rice husk fast pyrolysis in a conical spouted bed reactor
Jon Álvarez, Gartzen López, Maider Amutio et al. · Fuel · 2014 · 321 citations
Life Sciences, Chemical Engineering, Biochemical Engineering +15
Upgrading of pyrolysis bio-oil using nickel phosphide catalysts
Natsume Koike, Sou Hosokai, Atsushi Takagaki et al. · Journal of Catalysis · 2015 · 161 citations · Full text