EngineeringMaterials SciencePetroleum EngineeringCorrosion ScienceOffshore StructuresWell IntegrityCorrosion Of Offshore StructuresStress Corrosion CrackingSubsea CorrosionTubing IntegrityMicrostructureStress Corrosion Cracking In SeawaterTubing CorrosionTubing CrackingTubing Damage MechanismsTubing Failure AnalysisTubing RepairTubular Joint Connections
Abstract This paper describes the investigation of a high strength 25Cr Super Duplex tubing failure on the Shearwater HP/HT platform in the Central North Sea. Examination and analysis work conducted is described; conclusions as to the most likely cause of the failure are presented, along with recommendations on avoiding similar failures. On 23rd March 2003, the production tubing in the Shearwater well SW05 failed after the well had been re-perforated. After work to repair a leaking wellhead valve on the B annulus, the production casing seal assembly also failed, allowing communication between the A and B annuli. After killing and securing the well the completion was recovered. A10 ft (3 m) tubular joint of 7” 38 lb/ft 25Cr Super Duplex tubing had split along its entire length and parted close to its connection to the tubing hanger. The initiation site of the failure was found to have originated from a hardened area of modified microstructure, under a ground region on the outside surface of the tubular. Extensive examination and testing concluded that the failure was most likely caused by Chloride Stress Corrosion Cracking (CSCC). The paper describes the investigation that lead to that conclusion.