Optical, morphological, and electrical properties of P3HT: SiNWs nanocomposite deposited on flexible substrate: effect of SiNWs concentration

Hamza Saidi, Walid Aloui, Abdelaziz Bouazizi, Beatriz Romero Herrero, F. Saidi

Materials Research Express · 2017 · 13 citations · 27 references

Concepts

Abstract

The following flexible structure PET-ITO/PEDOT:PSS/P3HT:SiNWs/Al has been fabricated. The effect of the concentration of silicon nanowires (SiNWs) on the transfer and transport properties of the elaborated hybrid nanocomposite P3HT:SiNWs is studied by photoluminescence (PL) and current–voltage measurements. From PL spectra, we conclude that lower SiNW concentration leads to a higher charge transfer rate. However, higher concentration leads to an increase in defects and aggregates. This result is correlated with SEM images and J-V measurement. According to the thermionic model, electric parameters such as ideality factor n and barrier height Фb were calculated. For the P3HT:SiNWs (1:1) ratio, barrier height and parallel resistance Rp were found to be 0.71 V and 6 KΩ, respectively.

References

27