Fusion Engineering and Design · 2017 · 31 citations · 5 references
EngineeringMaterials EngineeringNuclear EngineeringFinite Element AnalysisMechanical Behavior Of MaterialsNuclear MaterialsDivertor DesignDivertor EngineeringFracture MechanicsFracture ToughnessFusion Reactor MaterialsThermal DesignBrittle DamageBrittle FailureCrack InitiationCrackingCracksFatigue Crack InitiationLow-cycle FatigueTungsten Armor
Recent high heat flux (HHF) tests showed that the tungsten monoblock armor often suffered from deep cracking, when the applied HHF load approached 20 MW/m2. The deep cracks were initiated at the armor surface and grew toward the cooling tube. The deep cracking seemed not to affect the heat removal capability of tungsten divertor, as most of the cracks were perpendicular to the loading surface. However, the inherently unstable nature of brittle cracking may likely increase the risk of structural failure. In this work, three variants (reduction in width of armor, inverse trapezoid shape in the lower part and castellation) of full-W divertor armor design based on the ITER divertor design are proposed to mitigate deep cracking at 20 MW/m2. The temperature, stress and strain fields are simulated with finite element method. The possibilities of crack initiation and propagation are evaluated by calculating the low cycle fatigue lifetime and J-integrals, respectively. All three variants can mitigate deep cracking of tungsten armor.
5
Use of tungsten material for the ITER divertor
Takeshi Hirai, S. Panayotis, V. Barabash et al. · Nuclear Materials and Energy · 2016 · 337 citations · Full text
Conceptual design studies for the European DEMO divertor: Rationale and first results
J.-H. You, G. Mazzone, E. Visca et al. · Fusion Engineering and Design · 2015 · 135 citations · Full text