Nuclear Materials and Energy · 2016 · 337 citations · 29 references
EngineeringMaterials EngineeringMaterials ScienceMechanical Behavior Of MaterialsMetallurgyNuclear MaterialsDamage MechanicsDivertor DesignDivertor EngineeringFracture MechanicsFusion Reactor MaterialsHigh-temperature MaterialsAcceptance CriteriaCracksDivertor MaterialsHigh-heat-flux MaterialsHigh-heat-flux TestingLow-cycle FatigueMaterial Acceptance CriteriaTungsten Divertor Materials
Since the ITER divertor design includes tungsten monoblocks in the vertical target where heat loads are maximal, the design to protect leading edges as well as technology R&D for high performance armor-heat sink joint were necessary to be implemented. In the R&D, the availability of the technology was demonstrated by high heat flux test of tungsten monoblock components. Not systematically but frequently macro-cracks appeared at the middle of monoblocks after 20 MW/m2 loading. The initiation of such macro-cracks was considered to be due to cyclic exposure to high temperature, ∼2000 °C, where creep, recrystallization and low cycle fatigue were concerned. To understand correlation between the macro-crack appearance and mechanical properties and possible update of acceptance criteria in the material specification, an activity to characterize the tungsten monoblocks was launched.
29
Fatigue: A complex subject—Some simple approximations
S. S. Manson · Experimental Mechanics · 1965 · 1.3K citations · Full text
A full tungsten divertor for ITER: Physics issues and design status
R.A. Pitts, S. Carpentier, F. Escourbiac et al. · Journal of Nuclear Materials · 2013 · 776 citations
Assessment of tungsten for use in the ITER plasma facing components
Jim Davis, V. Barabash, A. Makhankov et al. · Journal of Nuclear Materials · 1998 · 341 citations