Natural SciencesMaterials SciencePhysicsCondensed Matter PhysicsElectronic MaterialsSemiconductor MaterialsAb Initio MethodsDensity Functional TheoryElectronic Band StructureThermal Properties Of MaterialsThermal Properties Of SemiconductorsThermoelectric MaterialsBand GapElectronic Band GapElectronic Band TheoryElectronic ConductivitySeebeck CoefficientSeebeck EffectThermoelectric PropertiesThermoelectric Transport Coefficients
We present the thermoelectric properties of Antimony Selenide (Sb 2 Se 3 ) obtained using first principles calculations. We investigated the electronic band structure using the FP-LAPW method within the sphere of the density functional theory. Thermoelectric properties were calculated using BoltzTrap code using the constant relaxation time (<mml:math xmlns:mml="http://www.w3.org/1998/Math/MathML" id="M1"><mml:mrow><mml:mi>τ</mml:mi></mml:mrow></mml:math>) approximation at three different temperatures 300 K, 600 K, and 800 K. Seebeck coefficient (<mml:math xmlns:mml="http://www.w3.org/1998/Math/MathML" id="M2"><mml:mrow><mml:mi>S</mml:mi></mml:mrow></mml:math>) was found to decrease with increasing temperature, electrical conductivity (<mml:math xmlns:mml="http://www.w3.org/1998/Math/MathML" id="M3"><mml:mi>σ</mml:mi><mml:mo>/</mml:mo><mml:mi>τ</mml:mi></mml:math>) was almost constant in the entire temperature range, and electronic thermal conductivity (<mml:math xmlns:mml="http://www.w3.org/1998/Math/MathML" id="M4"><mml:mi>κ</mml:mi><mml:mo>/</mml:mo><mml:mi>τ</mml:mi></mml:math>) increased with increasing temperature. With increase in temperature <mml:math xmlns:mml="http://www.w3.org/1998/Math/MathML" id="M5"><mml:mrow><mml:mi>S</mml:mi></mml:mrow></mml:math> decreased from 1870 μ V/K (at 300 K) to 719 μ V/K (at 800 K), electronic thermal conductivity increased from 1.56 × 10 15 W/m K s (at 300 K) to 3.92 × 10 15 W/m K s (at 800 K), and electrical conductivity decreased from 22 × 10 19 /Ω m s (at 300 K) to 20 × 10 19 /Ω m s (at 800 K). The thermoelectric properties were also calculated for different hole concentrations and the optimum concentration for a good thermoelectric performance over a large range of temperatures (from 300 K to 1000 K) was found for hole concentration around 10 19 cm −3 .
17
Topological insulators in Bi2Se3, Bi2Te3 and Sb2Te3 with a single Dirac cone on the surface
Haijun Zhang, Chao‐Xing Liu, Xiao‐Liang Qi et al. · Nature Physics · 2009 · 6.3K citations
Ultralow thermal conductivity and high thermoelectric figure of merit in SnSe crystals
Li‐Dong Zhao, Shih‐Han Lo, Yongsheng Zhang et al. · Nature · 2014 · 5.1K citations
Optical Processes in Semiconductors
J. I. Pánkové, D. A. Kiewit · Journal of The Electrochemical Society · 1972 · 4.6K citations