Growth and Crystallization of TiO<sub>2</sub> Thin Films by Atomic Layer Deposition Using a Novel Amido Guanidinate Titanium Source and Tetrakis-dimethylamido-titanium

Marcel Reiners, Ke Xu, Nabeel Aslam, Anjana Devi, Rainer Waser, Susanne Hoffmann‐Eifert

Chemistry of Materials · 2013 · 86 citations · 45 references

Concepts

Abstract

We studied the growth of TiO 2 by liquid injection atomic layer deposition (ALD) utilizing two different amide-based titanium sources, tetrakis-dimethylamido-titanium [(NMe 2 ) 4 -Ti, TDMAT] and its recently developed derivative, tris-(dimethylamido)-mono-( N, N ′-diisopropyl-dimethyl-amido-guanidinato)-titanium {[(N-iPr) 2 NMe 2 ]Ti(NMe 2 ) 3, TiA 3 G 1 }, with water vapor as counterreactant. A clear saturation of growth with an increasing precursor supply was found for TDMAT between 150 and 300 °C and for TiA 3 G 1 between 150 and 330 °C. Representative growth per cycle (GPC) values at 250 °C were 0.041 and 0.044 nm/cycle, respectively. Compared to that of TDMAT, ALD of TiA 3 G 1 exhibited a significantly higher stability in the GPC values up to 300 °C coinciding with an improved temperature stability of the precursor. Both processes showed a minimum of the growth rate as a function of temperature. In all cases, the residual carbon and nitrogen contents of the TiO 2 films were <3 atom %. Conformal growth was demonstrated on three-dimensional pinhole structures with an aspect ratio of around 1:30. Deposition temperatures of ≤200 °C led to quasi-amorphous films. At higher growth temperatures, the anatase phase developed, accompanied by the brookite and/or the rutile phase depending on process conditions, deposition temperature, and film thickness.

References

45