The Journal of Physical Chemistry C · 2010 · 16 citations · 22 references
Natural SciencesMaterials EngineeringMaterials ScienceElectronic MaterialsMetallic MaterialsThin FilmsDefects In Electronic MaterialsMetal-semiconductor ContactsMetalsSurface PhysicsThin Film AnnealingThin Film Electrical PropertiesAnnealing EffectsContact DegradationGrain DensityOhmic ConductionOhmic MaterialsSchottky BarriersSchottky ContactsSchottky Defects
Au contacts were fabricated on Mg 0.27 Zn 0.73 O thin films that had been annealed by different processes. For the as-grown and vacuum annealed thin films, the Au/MgZnO contacts show ohmic behavior. For the thin film annealed in vacuum followed by in air, the contact shows current−voltage curve with Schottky characteristics and ultraviolet photo response at 0 V bias. This Schottky contact is attributed to the decrease of grain boundary density during vacuum annealing and the repair of defects during succedent annealing in air. At 5 V bias, the UV/visible (330 nm/440 nm) reject ratio of the Schottky detector reaches 4 orders of magnitude, obviously higher than the non-Schottky ones based on the as-grown MgZnO thin films and the vacuum annealed ones.
22
Semiconductor ultraviolet detectors
Manijeh Razeghi, Antoni Rogalski · Journal of Applied Physics · 1996 · 1.5K citations