Metastable Au<sub><i>x</i></sub>Rh<sub>100–<i>x</i></sub> Thin Films Prepared by Pulsed Laser Deposition for the Electrooxidation of Methanol

Régis Imbeault, David Reyter, Sébastien Garbarino, Lionel Roué, Daniel Guay

The Journal of Physical Chemistry C · 2012 · 18 citations · 36 references

Concepts

Abstract

Metastable Au x Rh 100– x thin films were prepared by crossed beam pulsed laser deposition on two different substrates. High kinetic-energy deposition conditions were used (0.1 Torr He, 5.5 cm target-to-substrate distance). The films were characterized by X-ray diffraction and X-ray photoelectron spectroscopy, and their electrocatalytic activities for the electrooxidation of methanol were assessed by linear sweep voltammetry in 1 M NaOH. All films are made of a single fcc phase compound. For 40 < x < 85 at %, the lattice parameter deviates slightly from that expected from Vegard’s law. The XRD patterns of Au x Rh 100– x /C and Au x Rh 100– x /Si did not evolve over a period of 1 year, indicating that the solid solution is kinetically stable. However, as expected from the Au–Rh binary phase diagram, heat treatment of Au 50 Rh 50 /C at 500 °C in Ar during 24 h leads to decomposition of the metastable fcc phase and the formation of Rh and Au. X-ray photoelectron spectroscopy revealed that the Au surface composition closely follows the Au bulk content. The binding energy difference between the Rh 3d 5/2 and Au 4f 7/2 core level peaks shifts from 223.3 to 222.4 eV as x is increased from 5 to 95, indicating that a surface alloy is formed between Au and Rh. In the presence of methanol, Au x Rh 100– x /C with x = 25, 50, and 75 shows a methanol oxidation peak (a 2 ) in a potential region (ca. −0.12 V vs Hg/HgO), where pure Au and Rh do not exhibit any electrocatalytic activity for methanol oxidation. The current of peak a 2 increases with the methanol concentration. The formation of a surface alloy significantly improves the electrocatalytic activity for methanol oxidation by providing OH – species at lower potential (by 400 mV) compared with pure Au.

References

36