AIP conference proceedings · 2014 · 16 citations · 2 references
Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsElectronic MaterialsSemiconductor MaterialsPhotovoltaic MaterialsSemiconductor Device MaterialsSemiconductor Thin FilmsSolar Cell MaterialsSolar CellsThin Film Electrical PropertiesBand GapBarium Titanate CeramicsEnergyEnergy Band GapSol-gel ProcessingSolar Cell CharacterizationSolar Cell FabricationSpin Coating
Growth of Ba0.5Sr0.5TiO3 (BST) 1 M thick films are conducted with variation of annealing hold time of 8 hours, 15 hours, 22 hours, and 29 hours at a constant temperature of 850 0 C on p-type Si (100) substrate using sol-gel method then followed by spin coating process at 3000 rpm for 30 seconds. The BST thick film electrical conductivity is obtained to be 10 -5 to10 -4 S/cm indicate that the BST thick film is classified as semiconductor material. The semiconductor energy band gap value of BST thick film based on annealing hold time of 8 hours, 15 hours, 22 hours, and 29 hours are 2.58 eV, 3.15 eV, 3.2 eV and 2.62 eV, respectively. The I-V photovoltaic characterization shows that the BST thick film is potentially solar cell device, and in accordance to annealing hold time of 8 hours, 15 hours, 22 hours and 29 hours have respective solar cell energy conversion efficiencies of 0.343%, 0.399%, 0.469% and 0.374%, respectively. Optical spectroscopy shows that BST thick film solar cells with annealing hold time of 8 hours, 15 hours, and 22 hours absorb effectively light energy at wavelength of 700 nm. BST film samples with annealing hold time of 29 hours absorb effectively light energy at wavelength of 700 nm. The BST thick film refraction index is between 1.1 to 1.8 at light wavelength between 370 to 870 nm.
2