Chemistry of Materials · 1998 · 54 citations · 25 references
Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsMaterials ChemistryThin FilmsDielectric CeramicsDielectricsElectrical Properties Of CeramicsThin Film AnnealingThin Film Electrical PropertiesThin-film MaterialsBarium TitanateCeramic DielectricsDielectric ConstantPyrolysisResistivitySpray PyrolysisThin Film CeramicsThin-film Dielectrics
Thin-film BaTiO 3 has been prepared for the first time by spray pyrolysis. Both smooth and highly porous films were deposited depending on deposition temperature and rate. As-deposited films contained an unidentified, low-symmetry barium titanate modification. Annealing at 500−900 °C converted the films to the cubic phase, while annealing at 1000 °C produced the tetragonal phase and an increase in the grain size. As-deposited and annealed films were highly dielectric with DC resistivity in the 10 10 −10 12 Ω·cm range. AC resistivity decreased with frequency following a power-law dependence with an exponent of −0.6 to −0.7. Both resistivity and capacitance remained stable at temperatures to 400 °C. The effective dielectric constant (20−25 at 10 kHz) was possibly determined by amorphous grain-boundary region with high density of traps.
25