Transactions of The Electrochemical Society · 1935 · 12 citations · 0 references
Natural SciencesMaterials EngineeringMaterials ScienceElectrochemistryMetallurgySurface ScienceAlloysElectrode MaterialsAdditive Effects On DepositionConcentrationConcentration DependenceTin DepositsTin Metallurgy
Lactic acid appears to be the best addition agent in the plating of tin from alkaline stannate baths. A concentration of 0.6 g./L. gives the best deposit. Malic acid, ethylene glycol, and tartaric acid also worked well, although they did not give quite as good deposits as did lactic acid. Other additions studied were sodium perborate, sodium biborate, casein, glucose, aloin, starch, triethanol amine, and glycerine. Increasing the alkalinity of the bath reduces the weight of the deposit. Varying the concentration of the addition agent has an effect on the weight of the deposit. With some addition agents, a certain concentration of the addition agent causes a maximum weight of deposit to form, while with other addition agents, a deposit of minimum weight forms.