Science and Technology of Welding & Joining · 2005 · 23 citations · 4 references
EngineeringMaterials EngineeringMaterials ScienceMetallic MaterialsMetallurgyUltrasoundAlloysJoint StrengthSteel MaterialsUltrasonic WeldingUltrasonicsUltrasound InstrumentationAluminium AlloysAluminum Alloy JoiningBond StrengthFiller MaterialsInterfacial Bond FormationMetal Ultrasonic WeldingSteelsUltrasonic Treatment
Carbon steel is joined to aluminium using the ultrasonic brazing method with Zn–Al filler at 663 K, employing different ultrasound application times. Different reaction layers could be observed at the interface, containing compounds such as FeAl 3 , Fe 2 Al 5 , Fe 3 Al, and FeAl, and solid solutions such as Fe–Zn and Zn–Al. For shorter ultrasound application times, formation of the aluminium rich Fe–Al compounds occurred; conversely, after longer ultrasound times formation of the iron rich Al–Fe compounds occurred, which improves the joint bond strength. The maximum bond shear strength of 127 MPa was obtained for an Al–steel joint brazed at 663 K with 3 s ultrasound application time. Extending the ultrasound time beyond 3 s caused the formation of FeAl compound, which decreased the joint bond strength; however, the strength of the joints remained at a higher level than that obtained with FeAl 3 and Fe 2 Al 5 .
4
International Institute of Welding
R. B. McCauley · Indian Welding Journal · 1972 · 91 citations
Engineering, Industrial Engineering, Mechanical Engineering +8
Msanori Yasuyama, Kazuhiro Ogawa, Takao Taka · QUARTERLY JOURNAL OF THE JAPAN WELDING SOCIETY · 1996 · 57 citations · Full text