IEEE Transactions on Magnetics · 1997 · 28 citations · 11 references
Natural SciencesMaterials EngineeringMaterials ScienceMagnetic MaterialsMaterials CharacterizationThin FilmsMagnetic Thin FilmsMetalsThin Film AnnealingThin Film Magnetic PropertiesThin-film MaterialsAmorphous Magnetic FilmsCoercivityCrystallographic TextureMagnetic PropertiesThin Film MagnetismThin-film Magnetic MaterialsUnderlayersX-ray Diffraction Analysis
A series of NdFeB (Nd/sub 12/Fe/sub 82/B/sub 6/) films of different thicknesses were r.f. sputtered on 1000 /spl Aring/-thick Pt underlayers for information storage application. The perpendicular coercivity has a maximum of 3000 Oe for a 1000 /spl Aring/ - thick film annealed at 625/spl deg/C for fifteen minutes. By using Transmission Electron Microscopy (TEM) we have found that the film is tetragonal with an additional fcc structure. The crystallographic texture is established during annealing at 625/spl deg/C. The TEM micrographs show some voids and a grain size in the range 30 to 50 nm. For films annealed at 700/spl deg/C for fifteen minutes, the voids disappeared and the grain size was found to be 100 nm. X-Ray Diffraction analysis of the annealed sample indicates that the NdFeB film is amorphous. Annealing at 625/spl deg/C produces the 2:15:1 phase in the films.
11
Anisotropic Nd–Fe–B thin-film magnets for milli-size motor
Shinji Yamashita, J. Yamasaki, M. Ikeda et al. · Journal of Applied Physics · 1991 · 172 citations · Full text
Natural Sciences, Materials Engineering, Materials Science +17
Micro patterning of thin NdFeB films
H. Lemke, Thomas C. Lang, T. Göddenhenrich et al. · Journal of Magnetism and Magnetic Materials · 1995 · 57 citations
Natural Sciences, Materials Engineering, Materials Science +14