Changes in the Lattice Constants of Thin-Film LiCoO[sub 2] Cathodes at the 4.2 V Charged State

Yong Jeong Kim, Eung-Kyu Lee, Hyemin Kim, Jaephil Cho, Young Whan Cho, Byungwoo Park, Seung M. Oh, Jong Kyu Yoon

Journal of The Electrochemical Society · 2004 · 30 citations · 29 references

DOIFull text

Open access

Concepts

Abstract

The lattice constants of thin-film Li 1x CoO 2 cathodes at the 4.2 V charged states were influenced by various deposition conditions. Li 1x CoO 2 thin films yielding a strong 003 texture on a Pt or Au current collector, which were unheated during sputtering deposition and ex situ annealed, showed negligible lattice expansion at 4.2 V during the first charge. This is in contrast to the Li 1x CoO 2 powders exhibiting 3% c axis expansion at x 0.5 from 14.05 to 14.45 . The total energy of the constrained Li 0.5 CoO 2 lattice 0% c axis expansion obtained by a pseudopotential total-energy calculation was slightly higher than that of the relaxed one by 1.0 eV per 12 Li 0.5 CoO 2 or 80 meV/Li 0.5 CoO 2 ), indicating no difficulty of limited lattice expansion during the first cycle. However, splitting of the 009 diffraction peak was observed at 4.2 V as cycling proceeded: one has a lattice constant c of 14.01 0.05 as LiCoO 2 before charging, and the other has a lattice parameter of 14.40 0.05 , which is similar to the Li 0.5 CoO 2 powders. In contrast, the lattice constants c of the Li 1x CoO 2 thin films deposited at different conditions yielding a weak 003 texture expanded when first charged to 4.2 V, which is similar to that observed in the powder geometry.

References

29