Composition and Properties of Hot‐Pressed SiC‐AIN Solid Solutions

Robert Ruh, Avigdor Zangvil

Journal of the American Ceramic Society · 1982 · 165 citations · 7 references

Concepts

TL;DR

High‑density SiC‑AIN compositions were fabricated from powder mixtures by hot‑pressing in the 1700 °C to 2300 °C temperature range. At 2100 °C, a 2H SiC‑AIN solid solution formed from 35–100 wt % AlN, showed steep composition gradients (>10 %/µm), Vegard‑law lattice parameters, a linear decrease in microhardness with increasing AlN, and grain sizes that grew with temperature yet remained smaller than pure SiC or AIN, leading to low flexural strengths.

Abstract

High‐density SiC‐AIN compositions were fabricated from powder mixtures by hot‐pressing in the 1700° to 2300°C temperature range. At 2100°C, a 2H solid solution was found from =35 to 100 wt% AlN. The single‐phase solid solution samples had steep composition gradients of >10%/μm within the grains. Lattice parameters closely followed Vegard's law. For compositions with <35% AIN, multiphase assemblages were found. Increasing grain size was observed for increasing firing temperature for SiC and AIN. Grain size of the solid solutions was significantly smaller than for SiC or AIN fired to the same temperature. Microhardness values decreased linearly in the solid solution region with increasing AIN content. Flexural strengths of SiC and AIN decreased with increasing firing temperature and increasing grain size. The strengths of SiC, AIN, and the solid solutions were low for materials hot‐pressed at 2100°C.

References

7