New processable polyaromatic ether‐keto‐sulfones curable by intramolecular cyclization. XV

Shiow‐Ching Lin, C. S. Marvel

Journal of Polymer Science Polymer Chemistry Edition · 1979 · 13 citations · 5 references

Concepts

Abstract

Abstract New processable polyaromatic ether‐keto‐sulfones were prepared from 2,2′‐diiododiphenyl‐4,4′‐dicarbonyl dichloride (I), bis( p ‐phenoxybenzene)sulfone (II), isophthaloyl chloride (III), and diphenyl ether (IV) in Friedel–Crafts‐type polymerizations. In the most promising of the iodine‐containing polymers phenylacetylenyl groups were introduced in place of iodine. This polymer, with an initial monomer ratio of I:II:III:IV = 1:5:7:3, was further investigated. It is soluble in DMF, DMA, pyridine, and sulfuric acid. After curing it was insoluble in all solvents used and lost only 1.1% of its weight at 300°C when heated in air for three days. Hence in this cured state it has excellent chemical and thermal resistance. It can be cast into a film from solution in DMAc and a glass fiber laminate is readily prepared. The film is tough, transparent, and brown in color. The cured film is tougher than the uncured. The glass fiber laminate is also tough and fairly flexible. A distinct advantage of this type of polymer is its ready availability in relatively cheap raw materials. The phenylacetylenyl‐group‐containing polymer showed a transition temperature at 175°C and two exotherm peaks at 243 and 361°C which disappeared after curing in a DSC thermogram. Before and after curing this polymer displayed softening temperatures at 149 and 171°C, respectively, measured by a Vicat apparatus at a heating rate of 1°C/min. No melting temperatures up to 500°C were observed for any of the polymers in this study.

References

5