Journal of Applied Physics · 1993 · 17 citations · 8 references
Natural SciencesMaterials EngineeringMaterials ScienceMagnetic MaterialsMetallic MaterialsSolid State PhysicsAlloysAmorphous Magnetic MaterialsAmorphous MaterialsAmorphous SolidsFerromagnetic MaterialsMagnetostrictive MaterialsAmorphous AlloysAmorphous Magnetic AlloysAmorphous Magnetostrictive AlloysIntermetallic Magnetic CompoundsMagnetic AlloysMagnetostrictionSaturationSaturation Magnetization
RFe2 laves phase intermetallic compounds are promising materials for magnetostrictive applications. To obtain a larger magnetostriction in a low magnetic field, the influence of boron addition on the giant magnetostriction of an amorphous (SmFe2) (1−x) at. % B (x) at. % alloy has been examined. In the amorphous alloy, the saturation magnetostriction anomalously increases, while the saturation magnetization decreases with the increase in x. The highest saturation magnetostriction of −670×10−6 at 10 kOe and its effective magnetostriction of −490×10−6 at 0.3 kOe can be obtained for amorphous (SmFe2) 99.26 at. % B 0.74 at. % alloy. This effective giant magnetostriction obtained in a low magnetic field is larger than those reported in previous researches. I attribute this anomalous giant magnetostriction in a low magnetic field to the increment of elastic energy in the amorphous (SmFe2) (1−x) at. % B (x) at. % alloy.
8
Ferromagnetic phases of bcc and fcc Fe, Co, and Ni
V. L. Moruzzi, P. M. Marcus, Karlheinz Schwarz et al. · Physical review. B, Condensed matter · 1986 · 716 citations
The structure of glassy metallic alloys
D.E. Polk · Acta Metallurgica · 1972 · 304 citations
Natural Sciences, Materials Engineering, Materials Science +11
Splat cooling and metastable phases
H. Jones · Reports on Progress in Physics · 1973 · 265 citations
Natural Sciences, Materials Engineering, Materials Science +15