Journal of the American Ceramic Society · 2009 · 15 citations · 20 references
Natural SciencesMaterials EngineeringMaterials ScienceElectronic MaterialsMaterials ChemistryThin FilmsFerroelectric CeramicsFerroelectric MaterialsPiezoelectric CeramicsPiezoelectric MaterialsThin Film AnnealingThin-film MaterialsAnnealingAnnealing Temperature EffectsFilm ThicknessGrain Structure EvolutionIndium Tin Oxide Thin FilmsPiezoelectric PropertiesThin Film FerroelectricsThin-film Piezoelectrics
Bi 3.7 Nd 0.3 Ti 3 O 12 (BNT0.3) films were fabricated on indium tin oxide/glass substrates using a metal organic decomposition method at temperatures ranging from 500° to 650°C. A predominantly (100)‐oriented BNT0.3 film can be obtained even at 550°C. The growth mode of the predominantly (100)‐oriented BNT0.3 films fabricated by the sequential layer annealing method was discussed based on the structure evolution with the annealing temperature and the film thickness. The largest values of the remanent polarization and piezoresponse are observed in the BNT0.3 film annealed at 650°C, which can be ascribed to the grain growth and the release of the in‐plane residue tension stress.
20
Fatigue-free ferroelectric capacitors with platinum electrodes
C. A-Paz de Araujo, J. D. Cuchiaro, L. D. McMillan et al. · Nature · 1995 · 2.6K citations
Natural Sciences, Materials Engineering, Materials Science +14
Lanthanum-substituted bismuth titanate for use in non-volatile memories
Bae Ho Park, Bo Soo Kang, Sang Don Bu et al. · Nature · 1999 · 2.2K citations
Natural Sciences, Materials Engineering, Materials Science +13
R. Dat, June Key Lee, Orlando Auciello et al. · Applied Physics Letters · 1995 · 228 citations
Natural Sciences, Materials Engineering, Materials Science +17