Journal of The Electrochemical Society · 1984 · 38 citations · 0 references
Natural SciencesMaterials EngineeringMaterials ScienceMaterials ChemistryPhysical ChemistryThin FilmsAmorphous MaterialsAmorphous SolidsSemiconductor Thin FilmsThin Film Thermal PropertiesThin-film DepositionThin-film MaterialsAmorphous Thin FilmsBoron ChemistryDeposition RateDeposition Rate EffectsSubstrate Temperature Effects
Boron films of 0.1–1.5 μm thickness have been prepared on sapphire, silicon, and tantalum as substrates by the pyrolysis of decaborane in the molecular flow region (≦10−4 torr) and in a temperature range of 350°–1200°C. It is found that the deposition rate of the boron films is proportional to the decaborane partial pressure and the substrate temperature. Below 416°C, the deposition rate is given as a function of the substrate temperature and partial pressure of decaborane. This relation is