European Journal of Inorganic Chemistry · 2011 · 104 citations · 19 references
Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsElectronic MaterialsMaterials ChemistryDopingElectrical Properties Of CeramicsHeat ConductionSinteringThermal Properties Of MaterialsThermoelectric MaterialsAnnealingElectrical Conductivity EnhancementSeebeck CoefficientSeebeck EffectSpark Plasma SinteringThermal ConductivityThermoelectric PropertiesZintl Phases
Abstract Samples of Zintl phase YbCd 2– x Mn x Sb 2 (CaAl 2 Si 2 ‐type, space group P $\bar {3}$ m 1) were prepared by a solid‐state reaction followed by a suitable annealing and spark plasma sintering (SPS) for densification. Investigations were carried out on chemical substitution of Cd by Mn in order to optimize the thermoelectric figure of merit ZT in the solid solution system YbCd 2– x Mn x Sb 2 ( x = 0, 0.05, 0.1, 0.15, 0.2, 0.4, 0.6, 0.8, 1.0, 1.5 and 2.0). Seebeck coefficients, electrical and thermal conductivities of all the samples were measured in the temperature range 300–650 K. The presence of Mn ( x ≤ 0.2) substantially reduces the thermal conductivity and enlarges the Seebeck coefficient, meanwhile decreasing the electrical conductivity to a certain degree. As the concentration of Mn ( x ) becomes higher than 1.0, the semimetallic nature ofYbCd 2– x Mn x Sb 2 changes to that of a semiconductor with the majority the carriers switching from holes to electrons. Of all the samples, polycrystalline YbCd 1.85 Mn 0.15 Sb 2 (p‐type charge carriers) shows the highest figure of merit ZT of 1.14 at 650 K.
19
Complex thermoelectric materials
G. Jeffrey Snyder, Eric S. Toberer · Nature Materials · 2008 · 11.1K citations
Thermoelectric Cooling and Power Generation
Francis J. DiSalvo · Science · 1999 · 3.2K citations