International Endodontic Journal · 2006 · 66 citations · 29 references
The group, restored with conventional amalgam, had the weakest resistance to fracture when compared with the bonded restorations. No statistically significant differences were found between the bonded amalgam and composite resin groups.
29
Effect of HEMA on bonding to dentin
N Nakabayashi, K Takarada · Dental Materials · 1992 · 378 citations
Dentin: microstructure and characterization.
Grayson W. Marshall · PubMed · 1993 · 283 citations
Tissue Engineering, Materials Science, Structural Variations +10
Fracture resistance of endodontically-treated premolars adhesively restored.
Pietro Ausiello, A.J. de Gee, Sandro Rengo et al. · PubMed · 1997 · 159 citations