Journal of the American Ceramic Society · 2000 · 23 citations · 31 references
Natural SciencesMaterials EngineeringMaterials ScienceMaterials ThermodynamicsSolid-state ChemistryThermodynamicsGlass MaterialsPhase TransitionsThermal Properties Of CeramicsThermal Properties Of MaterialsGlass TransitionGlass Transition BehaviorGlass Transition TemperatureGlass Transition ThermodynamicsHeat CapacityHeat Capacity ChangesStructural RelaxationThermal Resistance
The kinetics of enthalpy relaxation (recovery) at the glass transition in x K 2 O·(20− x )MgO·80TeO 2 glasses has been examined from heat capacity measurements using differential scanning calorimetry to clarify the features of the structural relaxation in ternary TeO 2 ‐based glasses. Ternary glasses such as 10K 2 O·10MgO·80TeO 2 show high thermal resistance against crystallization compared with binary glasses. The degree of fragility m estimated from the activation energy for viscous flow E η and the glass transition temperature T g is m = 55–62, indicating a fragile character in TeO 2 ‐based glasses. Large heat capacity changes of 43.1–48.2 J·mol −1 ·K −1 are also observed at the glass transition. The activation energy for enthalpy relaxation Δ H is evaluated from the cooling rate dependence of the limiting fictive temperature, and values of Δ H = 897–1268 kJ·mol −1 are obtained. Negative deviation from additivity in Δ H is also observed. Values of the Kovacs–Aklonis–Huchinson–Ramos (KAHR) parameter θ estimated from Δ H and T g are 0.33–0.42 K −1 . It has been proposed that ternary glasses have more homogeneous and constrained glass structure compared with binary glasses.
31
Nonexponential relaxations in strong and fragile glass formers
R. Böhmer, K. L. Ngai, C. Austen Angell et al. · The Journal of Chemical Physics · 1993 · 2.4K citations
Natural Sciences, Materials Engineering, Materials Science +15
Enthalpy relaxation and recovery in amorphous materials
Ian M. Hodge · Journal of Non-Crystalline Solids · 1994 · 1.2K citations