Structural Dependence of Strain Gauge Effect and Surface Resistivity for Thin Gold Films

Michael R. Neuman, William G. Sutton

Journal of Vacuum Science and Technology · 1969 · 28 citations · 0 references

Concepts

Abstract

Gold films of 80 to 500 Å thickness were deposited onto 6-mil-thick glass substrates, and continuous measurement of electrical and mechanical properties pertinent to the use of a film as a strain gauge element were made in situ. Gauge factors of greater than 100 for films that are less than 100 Å thick have been observed. These are over a factor of 20 greater than reported foil bulk values. The temperature coefficients of resistance for these high-gauge factor films were negative and their microstructure consisted of isolated islands. Increasing the island size and joining of islands, such as occurs in annealing, caused the gauge factor to decrease for films having the same surface resistivity. Straining and relaxing films up to 16 000 times resulted in drift in most specimens although there was no observable microstructure change. Films having high initial surface resistivities and gauge factors drifted to higher values upon cycling, while those with relatively low initial values dropped upon cycling. Surface passivation by silicon monoxide films did not change the film structure, but did increase the resistivity and decrease the gauge factor.