Journal of the American Ceramic Society · 2011 · 53 citations · 23 references
Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsCeramicsMaterials ChemistryDielectric CeramicsElectrical Properties Of CeramicsFerroelectric CeramicsPiezoelectric CeramicsPiezoelectric MaterialsSinteringElectrical CeramicsElectromechanical CouplingGrain Size ImprovementLead-free Piezoelectric CeramicsLead-free PiezoelectricsPiezoelectric EffectSintering BehaviorSintering Reactions
The 0.95(K 0.5 Na 0.5 NbO 3 )–0.05Li(Nb 0.5 Sb 0.5 )O 3 doped with 0.8 mol% copper oxide (CuO) lead‐free piezoelectric ceramics were synthesized by conventional solid‐state reaction route. The introduction of CuO could significantly improve the sinterability of 0.95(K 0.5 Na 0.5 NbO 3 )–0.05Li(Nb 0.5 Sb 0.5 )O 3 ceramics. The grain size of the specimen was considerably decreased due to the formation of a large amount of liquid phase when the sintering temperature exceeded 960°C. The piezoelectric constant ( d 33 ), planar electromechanical coupling ( k p ), and dielectric constant ( ) values increased with increasing relative density and grain size. The improved piezoelectric and dielectric properties of d 33 =207 pC/N, k p =44%, tan δ=0.0137, Q m =320, and =340 can be obtained for specimens sintered at 960°C for 2 h.
23