Piezoelectric and Dielectric Characteristics of Single-Crystal Barium Titanate Plates

A.H. Meitzler, H. L. Stadler

Bell System Technical Journal · 1958 · 19 citations · 4 references

Concepts

Abstract

The dielectric constant of c-domain barium titanate single-crystal plates has been measured as a function of their average polarization, using ac voltages much smaller than the coercive voltage. As has been found previously, the dielectric constant at frequencies below thickness fundamental resonance has a minimum at zero average polarization. However, at frequencies well above thickness resonance the dielectric constant has a maximum at zero polarization. The variation is about 25 per cent from minimum to maximum in both frequency ranges. In both frequency ranges the conductance is highest at zero polarization. The piezoelectric output voltage of a BaTiO <inf xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">3</inf> single crystal subjected to a recurrent strain pulse of constant amplitude has been found to be approximately, but not exactly, proportional to its average polarization. There appears, in fact, to be a distinct hysteresis in the dependence.

References

4