Journal of Synchrotron Radiation · 2010 · 13 citations · 27 references
Natural SciencesChemical EngineeringMaterials ScienceCatalysisInorganic ChemistryMetallurgyCatalyst CharacterizationCatalyst StabilityCatalytic MaterialsCatalytic Reaction EngineeringIndustrial Catalytic ProcessesMetal SulfidesChamber Pressure EffectsCoordination Number AnalysisCoordination Number DeterminationHydrodesulfurizationMetal Oxide CatalystsSupported Hydrodesulfurization Catalysts
Ni species on the spent NiMo catalyst from ultra-deep hydrodesulfurization of gas oil in a commercial plant were studied by Ni K-edge EXAFS and TEM measurement without contact of the catalysts with air. The Ni-Mo coordination shell related to the Ni-Mo-S phase was observed in the spent catalyst by quasi in situ Ni K-edge EXAFS measurement with a newly constructed high-pressure chamber. The coordination number of this shell was almost identical to that obtained by in situ Ni K-edge EXAFS measurement of the fresh catalyst sulfided at 1.1 MPa. On the other hand, large agglomerates of Ni(3)S(2) were observed only in the spent catalyst by quasi in situ TEM/EDX measurement. MoS(2)-like slabs were sintered slightly on the spent catalyst, where they were destacked to form monolayer slabs. These results suggest that the Ni-Mo-S phase is preserved on the spent catalyst and Ni(3)S(2) agglomerates are formed by sintering of Ni(3)S(2) species originally present on the fresh catalyst.
27
Deactivation of hydroprocessing catalysts
Edward Furimsky · Catalysis Today · 1999 · 725 citations
Structure of poorly crystalline MoS2 — A modeling study
K. S. Liang, Russell R. Chianelli, F. Z. Chien et al. · Journal of Non-Crystalline Solids · 1986 · 187 citations