Self‐Diffusion of Er and Hf in Polycrystalline Er <sub>2</sub> O <sub>3</sub> ‐Stabilized HfO <sub>2</sub>

Roland Tesch, C. D. WIRKUS, M. F. BERARD

Journal of the American Ceramic Society · 1982 · 12 citations · 14 references

Concepts

Abstract

Tracer self‐diffusion coefficients for Er and Hf were measured in polycrystalline Er 2 O 3 ‐stabilized HfO 2 (fluorite phase) at compositions between 10 and 40 mol% Er 2 O 3 and temperatures between 1700° and 2033°C. In some instances, grain‐boundary coefficients were also determined. The Hf volume coefficients were generally slightly smaller than Er coefficients, but neither showed a strong composition dependence, a finding most likely attributable to extensive clustering of charged defects which apparently rendered a large proportion of the “notional” defects essentially immobile. The activation energies for volume coefficients were very large, ranging from 630 to 760 kJ‐mol −1 , and generally decreased with increasing Er 2 O 3 content.

References

14