Journal of Biomedical Materials Research · 1998 · 42 citations · 31 references
Natural SciencesBioengineeringBiomedical EngineeringBiocompatibilityBiomaterialsTissue EngineeringBarrier MembranesBiodegradable BiomaterialsBiodegradable PolymersBiodegradationPolymeric BiomaterialsPolymeric MembranesBiodegradable Barrier FilmsBiodegradable Barrier MaterialsBiodegradable MembranesPolymer Barrier FilmsPolymer Barrier MaterialsPolymer ImplantsPolymeric Implant MaterialsPolymeric Implants
Biodegradable barrier films were made by coagulating a solution of poly(DL-lactide) in N-methyl-2-pyrrolidone on porous polyethylene pads wetted with saline solution. The semisolid films were cut into 10 x 10 mm barriers and implanted subcutaneously in rabbits. At monthly intervals, the polymer implant sites were compared histologically to those implanted with USP negative control plastic. The polymer films were retrieved from the surrounding tissue, dried, weighed, and the changes in molecular weight determined using gel permeation chromatography. The molecular weight of the polymer decreased at a relatively constant rate over 5 months; however, no significant mass loss occurred until 5 months postimplantation. Also, no distinct histological differences were noted between the polymer barrier and the control plastic sites until 6 months when histiocytes and multinucleated giant cells showed a modest increase around fragmented polymer films. Similar barrier films also were fitted over naturally occurring buccal dehiscence defects in beagle dogs and the tissue sites compared histologically at 6 months to sham-operated control sites. New bone and dense connective tissues closely approximated segments of the remaining polymer and demonstrated the biocompatibility of the biodegradable films. Histomorphometric analyses of treated sites compared to sham controls showed that the polymer barrier is effective in promoting bone and cementum regeneration in periodontal defects in dogs.
31
New attachment following surgical treatment of human periodontal disease
Sture Nyman, Jan Lindhe, Thorkild Karring et al. · Journal Of Clinical Periodontology · 1982 · 1.1K citations
Hydrolytic degradation of devices based on poly(dl-lactic acid) size-dependence
Ilaria Grizzi, Henri Garreau, Suming Li et al. · Biomaterials · 1995 · 860 citations
Natural Sciences, Materials Engineering, Materials Science +14
New attachment formation as the result of controlled tissue regeneration
Jan Gottlow, Sture Nyman, Thorkild Karring et al. · Journal Of Clinical Periodontology · 1984 · 732 citations